Studi Eksperimental Pengaruh Type Gating System Terhadap Mechanical Properties Dan Mikrostruktur Pada Pengecoran Aluminium A356 – SiC Menggunakan Metode Stir Casting
DAFTAR PUSTAKA
Aditya wendy dkk, 2011 “ Analisa Pengaruh Variasi Pembebanan Terhadap aju
Keausan Bahan Aluminium Sekrap dan Al-Si dengan menggunakan Alat Uji
Keausan Tipe Pin On The Disk”. Departemen Teknik Mesin, Fakultas
Teknik, Universitas Sumatera Utara. Medan
Anilkumar,HC,dkk,2010, “ Mechanical Properties of Aluminium Alloy (Al6061)
Composites”, International Journal of Mechanical and Materials Engineering
(IJMME), Vol.6 (2011), No.1, 41-45
Aqida, SN, dkk, 2010, “ The Effects of Stirring Speed and Reinforcement Perticles
on Porosity Formation in Cast MMC” Jurnal Mekanikal, 16, 22-30.
ASM International, 2004, “ ASM Metal Handbook Composites”, United State of
America
ASTM G99-04, 2004, “Standard Test Method for Wear Testing with a Pin-on
Disk
Apparatus”. Philadelphia, PA : American Society for Testing and
Materials.
Douglas M. Considin P. E., 1983. “Scientific Encyclopedia”, Australia, Van Mostran
Reinold Company.
Graille, J., Lozano, P., Pioch,D. & Geneste,p. 1985. “ Essais d’alcoolsye d’huiles
Vegetales avec des Catalyseurs Naturels pour la Production de Carburants
Diesel. Oleagineux, 40(5) : 271-276.
Hafizh Abdul, dkk 2009. “Aluminum Murni dan Paduannya” Departemen Teknik
Pertanian, Fakultas Teknologi Pertanian, Institut Pertanian Bogor.
Hartomo, A. J,1992,” Komposit Metal”. Yogyakarta: Andi Offset
Hashim, J, 2001, “The Production of Cast Metal Matrix Composite by A Modified
Stir Casting Method”, Jurnal Teknologi, Universiti Teknologi Malaysia.
Ipung Kurniawan., Amat Umron, 2011. “Karakterisasi Blok Rem Kereta Api
Berbahan Al-Sic Berdasarkan Komposisi Material”. Infotekmesin Volume
3, Jurnal, Cilacap.
Jamil, dkk, 2011. “Pengaruh Putaran Terhadap Laju Keausan Al-Si Alloy
Menggunakan Metode Pin On Disk Test”. Jurnal Dinamis,Volume.II,
No.8,Januari 2011 ISSN 0216-7492
81
Kainer, K. U., 2006, “Metal Matrix Composites”, Wiley-VCH Verlag GmbH &
Co. KgaA, Weinheim, Chap. 1.
Khairul Sakti., 2009. “ Pembuatan Komposit Metal Al Alloy Nano Keramik SiC
dan Karakterisasinya”. Tesis. Sekolah Pascasarjana. USU Medan.
Kirk, R.E dan Othmer, D.F. 1981. “ Encyclopedia of Chemical Engineering
Technology”. New York : John Wiley and Sons Inc.
Meena, K. L., Manna, A., Banwait, S. S. dan Jaswanti, 2013, “An Analysis of
Mechanical Properties of the Developed Al/SiC-MMC’s”, American Journal
of Mechanical Engineering, vol. 1, pp. 14-19.
Oliver, B, 2002, “Metal Matrix Composite (MMC’s) ”, Empa, Swiss Federal
Laboratories for Material Research and Testing . Dept Material and
technology. Swiss
PradeepSharma, Gulshan Chauhan, Neeraj Sharma . 2011 ”PRODUCTION OF
AMC BY STIR CASTING- AN OVERVIEW” International Journal of
Contemporary Practises Vol.2 Issue1
Rahmawati Sari Zulaina, 2010, “Analisis Pengaruh Sr Terhadap Ketahanan
Korosi pada Paduan Aluminium”, FT Universitas Indonesia, Jakarta
Silalah
Marzuki
dkk,
1997,
“Pembuatan
dan
Karakterisasi
Komposit
AI(6061)/SiC” Prosiding Pertemuan Ilmiah Sains Materi
Simanjutak, Albin Moniago dkk, 2013.” karakterisasi komposit matriks logam Al
-
SiC pada produk kanvas rem kereta api”. Departemen teknik mesin,
fakultas teknik, USU
Suparman, 2010. “ Sintetis Silika Karbida ( SiC ) dari Sekam Padi dan Karbon
Kayu dengan Metode Reaksi Fasa Padat”, ( Tesis ), IPB, Bogor, Hal 1-95
Surdia Tata, 1996. “ Teknik Pengecoran Logam”. PT. Pradnya Paramita, Jakarta
Surdia, Tata, Saito, S, 2006. Pengetahuan Bahan Teknik. Edisi kesembilan.
Jakarta: PT. Pradnya Paramita.
Suyanto, Sulardjaka, Sri Nugroho.2014. “ Pengaruh komposisi
Mg dan SiC
Terhadap sifat Kekerasan Komposit AlSi-SiC yang Dibuat dengan Proses
Semi Solid Stir Casting” , Fakultas Teknik, Universitas Diponegoro
Tairov, Yu.M., V.F.Tsvetkov, in Handbook on electrotechnical Materials
eds.Koritskii,Yu.V., V.V. Pasynkov, B.M Tareev, vol 3 , sec.19,
82
“Semiconductor Compounds AIV BIV” , energomashizdat, leningrad, 1988,
446-471.
Widyastuti, 2009. “Rekayasa Proses”. Fakultas Teknik, Universitas Indonesia,
Jurnal, Jakarta.
Ye,H, 2002, “ An Overview of the Development of Al-Si-Alloy Based Material for
Engine Application”, JMEPEG, 12-288-297, ASM International.
Yuwono H.A, 2008, “Buku Panduan Praktikum Karakterisasi Material 1
Pengujian Merusak (Destruktive Testing)”, Departemen Metalurgi Dan
Material Fakultas Teknik Universitas Indonesia, Jakarta.
83
Aditya wendy dkk, 2011 “ Analisa Pengaruh Variasi Pembebanan Terhadap aju
Keausan Bahan Aluminium Sekrap dan Al-Si dengan menggunakan Alat Uji
Keausan Tipe Pin On The Disk”. Departemen Teknik Mesin, Fakultas
Teknik, Universitas Sumatera Utara. Medan
Anilkumar,HC,dkk,2010, “ Mechanical Properties of Aluminium Alloy (Al6061)
Composites”, International Journal of Mechanical and Materials Engineering
(IJMME), Vol.6 (2011), No.1, 41-45
Aqida, SN, dkk, 2010, “ The Effects of Stirring Speed and Reinforcement Perticles
on Porosity Formation in Cast MMC” Jurnal Mekanikal, 16, 22-30.
ASM International, 2004, “ ASM Metal Handbook Composites”, United State of
America
ASTM G99-04, 2004, “Standard Test Method for Wear Testing with a Pin-on
Disk
Apparatus”. Philadelphia, PA : American Society for Testing and
Materials.
Douglas M. Considin P. E., 1983. “Scientific Encyclopedia”, Australia, Van Mostran
Reinold Company.
Graille, J., Lozano, P., Pioch,D. & Geneste,p. 1985. “ Essais d’alcoolsye d’huiles
Vegetales avec des Catalyseurs Naturels pour la Production de Carburants
Diesel. Oleagineux, 40(5) : 271-276.
Hafizh Abdul, dkk 2009. “Aluminum Murni dan Paduannya” Departemen Teknik
Pertanian, Fakultas Teknologi Pertanian, Institut Pertanian Bogor.
Hartomo, A. J,1992,” Komposit Metal”. Yogyakarta: Andi Offset
Hashim, J, 2001, “The Production of Cast Metal Matrix Composite by A Modified
Stir Casting Method”, Jurnal Teknologi, Universiti Teknologi Malaysia.
Ipung Kurniawan., Amat Umron, 2011. “Karakterisasi Blok Rem Kereta Api
Berbahan Al-Sic Berdasarkan Komposisi Material”. Infotekmesin Volume
3, Jurnal, Cilacap.
Jamil, dkk, 2011. “Pengaruh Putaran Terhadap Laju Keausan Al-Si Alloy
Menggunakan Metode Pin On Disk Test”. Jurnal Dinamis,Volume.II,
No.8,Januari 2011 ISSN 0216-7492
81
Kainer, K. U., 2006, “Metal Matrix Composites”, Wiley-VCH Verlag GmbH &
Co. KgaA, Weinheim, Chap. 1.
Khairul Sakti., 2009. “ Pembuatan Komposit Metal Al Alloy Nano Keramik SiC
dan Karakterisasinya”. Tesis. Sekolah Pascasarjana. USU Medan.
Kirk, R.E dan Othmer, D.F. 1981. “ Encyclopedia of Chemical Engineering
Technology”. New York : John Wiley and Sons Inc.
Meena, K. L., Manna, A., Banwait, S. S. dan Jaswanti, 2013, “An Analysis of
Mechanical Properties of the Developed Al/SiC-MMC’s”, American Journal
of Mechanical Engineering, vol. 1, pp. 14-19.
Oliver, B, 2002, “Metal Matrix Composite (MMC’s) ”, Empa, Swiss Federal
Laboratories for Material Research and Testing . Dept Material and
technology. Swiss
PradeepSharma, Gulshan Chauhan, Neeraj Sharma . 2011 ”PRODUCTION OF
AMC BY STIR CASTING- AN OVERVIEW” International Journal of
Contemporary Practises Vol.2 Issue1
Rahmawati Sari Zulaina, 2010, “Analisis Pengaruh Sr Terhadap Ketahanan
Korosi pada Paduan Aluminium”, FT Universitas Indonesia, Jakarta
Silalah
Marzuki
dkk,
1997,
“Pembuatan
dan
Karakterisasi
Komposit
AI(6061)/SiC” Prosiding Pertemuan Ilmiah Sains Materi
Simanjutak, Albin Moniago dkk, 2013.” karakterisasi komposit matriks logam Al
-
SiC pada produk kanvas rem kereta api”. Departemen teknik mesin,
fakultas teknik, USU
Suparman, 2010. “ Sintetis Silika Karbida ( SiC ) dari Sekam Padi dan Karbon
Kayu dengan Metode Reaksi Fasa Padat”, ( Tesis ), IPB, Bogor, Hal 1-95
Surdia Tata, 1996. “ Teknik Pengecoran Logam”. PT. Pradnya Paramita, Jakarta
Surdia, Tata, Saito, S, 2006. Pengetahuan Bahan Teknik. Edisi kesembilan.
Jakarta: PT. Pradnya Paramita.
Suyanto, Sulardjaka, Sri Nugroho.2014. “ Pengaruh komposisi
Mg dan SiC
Terhadap sifat Kekerasan Komposit AlSi-SiC yang Dibuat dengan Proses
Semi Solid Stir Casting” , Fakultas Teknik, Universitas Diponegoro
Tairov, Yu.M., V.F.Tsvetkov, in Handbook on electrotechnical Materials
eds.Koritskii,Yu.V., V.V. Pasynkov, B.M Tareev, vol 3 , sec.19,
82
“Semiconductor Compounds AIV BIV” , energomashizdat, leningrad, 1988,
446-471.
Widyastuti, 2009. “Rekayasa Proses”. Fakultas Teknik, Universitas Indonesia,
Jurnal, Jakarta.
Ye,H, 2002, “ An Overview of the Development of Al-Si-Alloy Based Material for
Engine Application”, JMEPEG, 12-288-297, ASM International.
Yuwono H.A, 2008, “Buku Panduan Praktikum Karakterisasi Material 1
Pengujian Merusak (Destruktive Testing)”, Departemen Metalurgi Dan
Material Fakultas Teknik Universitas Indonesia, Jakarta.
83